Problems
|
Suggested Solutions
|
| Pitting or Foaming |
Further drying is required |
| Rough Appearance |
Check that proper screw is installed |
| Too Glossy |
Reduce screw speed
Reduce barrel temperature
Check that proper screw is installed |
| Surging |
Reduce screw speed
Eliminate screw cooling |
| Dimensional Variation |
Reduce screw speed |
| Black specks, Burning |
Check temperatures
Check quality and material of construction for surfaces in contact with melt
Check for streamlined, low inventory die/adapter
Clean out all burned or foreign material from die, adapter, and extruder
Check that proper screw is installed |
| Poor Impact and Physical Properties |
Check stock temperatures |